High-temperature structural intermetallics M Yamaguchi, H Inui, K Ito Acta materialia 48 (1), 307-322, 2000 | 1045 | 2000 |
Plastic deformation of MoSi2 single crystals K Ito, H Inui, Y Shirai, M Yamaguchi Philosophical Magazine A 72 (4), 1075-1097, 1995 | 184 | 1995 |
Physical and mechanical properties of single crystals of the T2 phase in the Mo–Si–B system K Ito, K Ihara, K Tanaka, M Fujikura, M Yamaguchi Intermetallics 9 (7), 591-602, 2001 | 174 | 2001 |
Effects of ZnSb and Zn inclusions on the thermoelectric properties of β-Zn4Sb3 LT Zhang, M Tsutsui, K Ito, M Yamaguchi Journal of Alloys and Compounds 358 (1-2), 252-256, 2003 | 142 | 2003 |
Mechanical properties of Mo5SiB2 single crystals K Ihara, K Ito, K Tanaka, M Yamaguchi Materials Science and Engineering: A 329, 222-227, 2002 | 121 | 2002 |
Formation of Ti diffusion barrier layers in thin Cu (Ti) alloy films S Tsukimoto, T Morita, M Moriyama, K Ito, M Murakami Journal of electronic materials 34, 592-599, 2005 | 93 | 2005 |
A new process for design and manufacture of tailor-made functionally graded composites through friction stir additive manufacturing A Sharma, V Bandari, K Ito, K Kohama, M Ramji, HS BV Journal of Manufacturing Processes 26, 122-130, 2017 | 91 | 2017 |
Ohmic contacts on silicon carbide: The first monolayer and its electronic effect Z Wang, S Tsukimoto, M Saito, K Ito, M Murakami, Y Ikuhara Physical Review B—Condensed Matter and Materials Physics 80 (24), 245303, 2009 | 86 | 2009 |
Complex macroscopic plastic flow arising from non-planar dislocation core structures JL Bassani, K Ito, V Vitek Materials Science and Engineering: A 319, 97-101, 2001 | 85 | 2001 |
Effects of in-doping on the thermoelectric properties of β-Zn4Sb3 M Tsutsui, LT Zhang, K Ito, M Yamaguchi Intermetallics 12 (7-9), 809-813, 2004 | 79 | 2004 |
Room temperature fracture toughness and high temperature strength of T2/Moss and (Mo, Nb) ss/T1/T2 eutectic alloys in the Mo–Si–B system K Ito, M Kumagai, T Hayashi, M Yamaguchi Scripta materialia 49 (4), 285-290, 2003 | 68 | 2003 |
Plastic deformation of MoSi2 and WSi2 single crystals and directionally solidified MoSi2-based alloys K Ito, T Yano, T Nakamoto, H Inui, M Yamaguchi Intermetallics 4, S119-S131, 1996 | 65 | 1996 |
Creep of single crystalline and polycrystalline T2 phase in the Mo–Si–B system T Hayashi, K Ito, K Ihara, M Fujikura, M Yamaguchi Intermetallics 12 (7-9), 699-704, 2004 | 62 | 2004 |
Plastic deformation of single crystals of Mo(Si, Al)2 with the C40 structure H Inui, M Moriwaki, K Ito, M Yamaguchi Philosophical Magazine A 77 (2), 375-394, 1998 | 61 | 1998 |
Electrical resistivity of polycrystalline Cu interconnects with nano-scale linewidth M Shimada, M Moriyama, K Ito, S Tsukimoto, M Murakami Journal of Vacuum Science & Technology B: Microelectronics and Nanometer …, 2006 | 60 | 2006 |
Effect of annealing ambient on the self-formation mechanism of diffusion barrier layers used in Cu (Ti) interconnects S Tsukimoto, T Kabe, K Ito, M Murakami Journal of electronic materials 36, 258-265, 2007 | 56 | 2007 |
Benefits of intermediate-layer formation at the interface of Nb/Cu and Ta/Cu explosive clads PK Parchuri, S Kotegawa, H Yamamoto, K Ito, A Mori, K Hokamoto Materials & Design 166, 107610, 2019 | 54 | 2019 |
Oxidation behavior of Mo–9Si–18B alloy pack-cemented in a Si-base pack mixture K Ito, T Murakami, K Adachi, M Yamaguchi Intermetallics 11 (8), 763-772, 2003 | 52 | 2003 |
Thermoelectric properties of Zn4Sb3 thin films prepared by magnetron sputtering LT Zhang, M Tsutsui, K Ito, M Yamaguchi Thin Solid Films 443 (1-2), 84-90, 2003 | 51 | 2003 |
Hydrogen absorption and desorption in a B2 single-phase Ti–22Al–27Nb alloy before and after deformation LT Zhang, K Ito, VK Vasudevan, M Yamaguchi Acta materialia 49 (5), 751-758, 2001 | 50 | 2001 |